1
1.
金冰 《火箭推进》2005,31(3):46-49
为了改善天然橡胶的热氧老化性能,试验了防老剂D提纯品和工业品对天然橡胶(NR)热氧老化性能的影响,测试了其热氧化诱导期、热失重、热老化的性能变化。结果表明:含杂少纯度高的防老剂D使天然橡胶的抗热氧老化得到改善。  相似文献   
2.
Simulated microgravity (SMG) can inhibit proliferation and enhance microcystin production of Microcystis aeruginosa. We investigated the role of nitric oxide (NO) in regulating the SMG induced changes of proliferation, photochemical system II photochemical activity, pigment, soluble protein and microcystin production in M. aeruginosa. M. aeruginosa was exposed to 0.1 mM sodium nitroprusside (SNP, NO donor) or 0.02 mM 2-(4-carboxyphenyl)-4, 4, 5, 5-tetramethylimidazoline-1-oxyl-3-oxide (c-PTIO, NO scavenger) alone or in combination with SMG for 48 h. SMG and SNP inhibited the growth of M. aeruginosa while c-PTIO had no effect on cell number. As to yield, the negative effect of SMG was augmented by SNP and suppressed by c-PTIO. The intracellular concentrations of chlorophyll a, carotenoid, phycocyanin, soluble protein and microcystin were increased by SMG after 48 h. The effects of SMG on these metabolic processes could be enhanced by SNP and be partly eliminated by c-PTIO. Moreover, SNP and c-PTIO only functioned in these biochemical processes under SMG, unlike in the regulation of cell proliferation and yield. These results showed that the effects of SMG could be enhanced by adding exogenous NO and be mitigated by scavenging endogenous NO, revealing the involvement of NO in the changes in biochemistry processes induced by SMG in M. aeruginosa.  相似文献   
3.
在比表面积相近的情况下,探讨白炭黑(Z125)及碳黑(N234)对天然橡胶(NR)和溶聚丁苯橡胶(S-SBR)硫化胶的抗割口增长能力及动态力学性能的影响.结果表明,Z125和N234对NR和S-SBR两种硫化胶的增强效果相差不大;NR硫化胶的抗割口增长能力明显好于S-SBR硫化胶;NR中填充Z125的抗割口增长能力好于N234且随疲劳次数的增加Z125的优势更加明显,而S-SBR中填充N234的抗割口增长能力好于Z125且两者的抗割口增长速率基本不随疲劳次数的增加而改变;Z125使NR和S-SBR硫化胶在0℃和70℃下的tanδ值分别低于N234增强相应硫化胶.  相似文献   
4.
介绍了用动态热机械分析仪测定天然橡胶(NR)硫化胶耐老化性能的原理及方法。通过测定胶料在160℃、恒温30min下的动态模量谱,来评估硫化胶的耐老化性能。同时测定硫化胶力学性能随老化时间的变化情况。结果显示:老化后储能模量减少,损耗模量和损耗因子tanδ总体呈增加趋势。力学性能随老化时间的延长呈先增加而后下降趋势。  相似文献   