排序方式: 共有20条查询结果,搜索用时 31 毫秒
1.
搭建薄液膜厚度测量与控制装置,采用微距参比电极后置法组建三电极体系,测量了厚度为100 μm的3.5wt% NaCl液膜下2A12铝合金、TC18钛合金和30CrMnSiNi2A高强钢的极化曲线和耦合体系的电偶电流;建立了基于薄壳电流分布的Comsol腐蚀仿真模型,得到了100 μm液膜下电极电位分布和电流密度分布图,通过对电极表面进行局部电流面积分计算得到了其电偶电流,对不同电极进行了面积的参数化扫描,讨论分析了不同面积比对于电偶电流的影响。结果表明:利用仿真模型得到的电偶电流值与试验值吻合较好,在2A12/30CrMnSiNi2A/TC18多电极体系中2A12充当阳极,TC18/30CrMnSiNi2A充当阴极,且阴阳极极性不随面积比的变化而发生转变,电偶电流主要集中在30CrMnSiNi2A与2A12之间,电偶电流与TC18面积呈线性关系,其对数与2A12和30CrMnSiNi2A面积的对数之间呈线性关系。利用建立的仿真模型对模拟搭接件大气腐蚀进行了仿真研究,仿真发现垫圈、2A12与30CrMnSiNi2A偶接接缝处及2A12与TC18偶接铆钉处电流密度分布更为集中,易发生腐蚀,与暴晒试验结果相符,说明该仿真模型对于多电极偶接的腐蚀分布具有很好的预测作用。 相似文献
2.
作者在H3PO4 C6 H1 1 NaO7体系中对TC10、TC3、TC1、TA2阳极氧化均能得到丰富色彩。研究表明 ,钛材的成分、电压、pH值、升压方式、氧化时间等对阳极氧化膜的颜色都有一定的影响 ,电压是影响氧化膜颜色的主要因素。此外 ,稀土元素铈和双氧水的加入能提高膜层的耐蚀性。 相似文献
3.
共轭羰基化合物以其高理论比容量与多电子参与等优势成为当前最具研究吸引力的有机电极材料之一。本文以苝四甲酸二酐(PTCDA)与尿素进行缩聚反应制备含有共轭多羰基单元的聚酰亚胺(PI),采用傅里叶转换红外线光谱分析仪(Fourier transform infrared spectroscope,FT-IR)、X射线衍射(X-ray diffraction,XRD)和扫描电子显微镜(Scanning electron microscope,SEM)等测试方法对其进行了表征,并将所制备的材料用作钠离子电池正极材料,研究了其在NaClO4/EC∶DMC和NaClO4/EC∶PC两种电解液体系中的嵌钠性质。结果表明:在NaClO4/EC∶PC中,PI的初始比容量最高,循环稳定性最好;在电流密度为0.3 C(1 C=118mA·g-1)时,循环100次后放电容量可达124 mAh·g-1。优异的电化学性质主要归因于NaClO4/EC∶PC高的离子电导率,因而PI在其中具有较好的动力学性能,进而表现出更优的电化学性能。 相似文献
4.
Effects of Hybrid Voltages on Oxide Formation on 6061 Al-alloys During Plasma Electrolytic Oxidation
Kai Wang Bon Heun Koo Chan Gyu Lee Young Joo Kim Sunghun Lee Eungsun Byon 《中国航空学报》2009,22(5):564-568
Plasma electrolytic oxidation (PEO) is carried out on 6061 Al-alloys in a weak alkaline electrolyte containing NaOH, Na2SiO3 and NaCl. Centered on the correlation of composition and structure, analyses by means of X-ray diffration (XRD), scanning electron microscope (SEM) and energy dispersive spectrometry (EDS) are conducted on the specimens, which have been PEO-treated under hybrid voltages of different direct current (DC) values (140-280 V) with constant alternate current (AC) amplitude (200 V). Attention is paid to the composition, properties and growth mechanism of oxide layers formed with hybrid voltages. Moreover, the main effects of DC value are discussed. Ceramic layers with a double-layer structure which combines hard outer and soft inner layers are found to be consist of α-Al2O3, γ-Al2O3 and mullite. With the DC values increasing, the growth of the ceramic layers tends to have increasingly obvious three-stage feature. 相似文献
5.
6.
7.
8.
The physiological and biochemical systems that regulate the level of each electrolyte in blood and other endogenous fluids, and the balance between the consumption and loss of fluid and electrolytes and the total fluid and electrolyte content of the body are significantly affected during hypokinesia (HK; diminished movement). Among the known effects of HK, the fluid and electrolyte deficiency has drawn a great interest due to the higher fluid and electrolyte deficiency with higher than lower fluid and electrolyte consumption. The impossibility of the body to use fluid and electrolytes, after the fluid and electrolyte deficiency has been established, has drawn the greatest interest. The fluid shifting to the thoracic region and the daily body rehydration are considered as the most effective methods to counteract fluid and electrolyte changes. To this end, the objective of this review was to report some of the findings in the fluid and electrolyte deficiency and fluid and electrolyte loss with fluid and electrolyte deficiency during prolonged HK. 相似文献
9.
Titanium and its alloys have found very wide application in aerospace due to their excellent characteristics although their processing is still a challenge. Electrochemical machining is an important issue in the fabrication of titanium and titanium alloys. Wire electrochemical machining (WECM) is mainly used for workpiece cutting under the condition of different thickness plates. It has a great advantage over wire electro-discharge machining, which is the absence of heat-affected zone around the cutting area. Moreover, the wire electrode in WECM could be used repetitively because it is not worn out. Thus, much attention has been paid to WECM. The effective way of removing electrolysis products is of importance to WECM. In this paper, the axial electrolyte flushing is presented to WECM for removing electrolysis products and renewing electrolyte. The Taguchi experiment is conducted to optimize the machining parameters, such as wire feedrate, machining voltage, electrolyte concentration, etc. Experimental results show that WECM with axial electrolyte flushing is a promising issue in the fabrication of titanium alloy (TC1). The feasibility of multi-wire electrochemical machining is also demonstrated to improve the machining productivity of WECM. 相似文献
10.
固态电池具有高能量密度和高安全性等潜力,是未来航天器电源的重要解决方案。本文利用原位聚合方法,制备了聚甲基丙烯酸甲酯(PMMA)凝胶/Li_(6.5)La_3Zr_(1.5)Ta_(0.5)O_(12)(LLZT)复合电解质。通过选择与陶瓷相润湿性好的甲基丙烯酸甲酯单体(MMA)进行原位聚合,改善了电解质内部陶瓷与凝胶的两相界面。室温下,此复合电解质具有6.6×10~(-4)S·cm~(-1)的离子导电率。进一步采用原位聚合法,制备了Li/复合电解质/Li对称电池。与非原位方法相比,原位聚合将电解质与金属锂的界面比电阻从1 572Ω·cm~2降至367Ω·cm~2,对称电池在0.085 mA·cm~(-2)下能够稳定循环400圈,显示出良好的循环稳定性。 相似文献