排序方式: 共有34条查询结果,搜索用时 359 毫秒
21.
Tzehan Chen Brian J. Chow Ying Zhong Meng Wang Rui Kou Yu Qiao 《Advances in Space Research (includes Cospar's Information Bulletin, Space Research Today)》2018,61(3):830-836
We report results from an experiment on high-pressure compaction of lunar soil simulant (LSS) mixed with 2–5?wt% polymer binder. The LSS grains can be strongly held together, forming an inorganic-organic monolith (IOM) with the flexural strength around 30–40?MPa. The compaction pressure, the number of loadings, the binder content, and the compaction duration are important factors. The LSS-based IOM remains strong from ?200?°C to 130?°C, and is quite gas permeable. 相似文献
22.
23.
张宗强%王玉林%万怡灶%李建%赵伟栋 《宇航材料工艺》2003,33(5):40-43
选择液态原位聚合法成功地制备出性能较好的三维编织碳纤维增强尼龙6复合材料(C3D/PA6)及三维编织芳纶纤维增强尼龙6复合材料(K3D/PA6);并对两种复合材料的力学性能进行了比较。研究发现,C3D/PA6的弯曲强度和弯曲模量均高于K3D/PA6,而K3D/PA6则比C3D/PA6具有更高的抗冲击强度和剪切强度。 相似文献
24.
颗粒增强钛基复合材料是一种重要的轻量化结构-功能一体化材料.在航空航天、空间技术、武器装备、能源和环境形势日益严峻的今天,这种轻质、高强、耐热颗粒增强钛基复合材料是航空航天技术、能源发展与交通运输等若干关键领域中不可替代的共性关键材料.从复合材料制备技术、基体和增强体选择,增强体分布设计,构型设计,热变形加工、超塑性加工、热处理、微观组织、力学性能以及工程应用方面综述了颗粒增强钛基复合材料的发展现状,提出了研究中存在的问题以及今后潜在的研究方向,为进一步推动和解决重大工程用复合材料大构件加工、精密成形制造的关键技术和装备提供指导,进而推动非连续颗粒增强钛基复合材料的深入发展. 相似文献
25.
26.
27.
28.
基于超精密机床的LVDT在线检测系统的研究 总被引:3,自引:0,他引:3
在线检测系统可以实现加工测量一体化,避免工件重复装卡对加工精度的影响。本文主要介绍了在线检测系统的构成、LVDT测头精度的校正以及球面测量面型精度的评估方法。 相似文献
29.
《中国航空学报》2021,34(11):131-139
In this paper fretting fatigue crack behavior in 1045 steel is studied by in-situ observation and finite element analysis. in-situ fretting fatigue experiments are conducted to capture real-time fretting fatigue crack formation and propagation process. The fretting fatigue tests under different load conditions are carried out, then the lifetime and fracture surface are obtained. The crack propagation rates under different loading conditions are measured by in-situ observations. With in-situ observation, crack initiation location and direction are analyzed. Finite element model is used to calculate J-integral which then is applied to fitting with experimental crack growth rate, and establishing crack growth rate model. From fitted S-N curve, it turns out that smaller load ratio leads to higher lifetime. Crack initiates slightly below the point equivalent to line contact of the contact surface in different test conditions, and crack direction shows no obvious relationship with load parameters. The established crack growth rate model well agrees with the test results. 相似文献
30.
采用原位红外光谱测试方法,通过对同一样品在连续变温过程中的红外谱图分析研究热固性酚醛树脂在固化过程中的化学结构变化和固化行为。结果表明:该热固性酚醛树脂的固化过程主要存在两种反应,羟甲基与酚环上的氢之间的取代反应、羟甲基与羟甲基间的缩合反应,且取代反应早于缩合反应发生。随红外曲线的实时变化可知,羟甲基的缩合反应过程中有醚键形成,而羰基的出现与醚键的消失有关。通过对酚醛固化过程中基团变化的连续实时监测,可为热固性酚醛树脂的固化工艺的确定提供科学依据。 相似文献