首页 | 本学科首页   官方微博 | 高级检索  
     检索      

固体发动机药柱的裂纹稳定性分析
引用本文:蒙上阳,唐国金,雷勇军.固体发动机药柱的裂纹稳定性分析[J].推进技术,2002,23(4):335-338.
作者姓名:蒙上阳  唐国金  雷勇军
作者单位:国防科技大学,航天与材料工程学院,湖南,长沙,410073
基金项目:国防科大预研基金项目 (JC0 2 0 1 0 0 4 )
摘    要:为了确定固体发动机药柱内表面裂纹在内压与轴向过载联合作用下的稳定性及最大允许裂纹深度,以翼锥药形的固体发动机为例,在危险截面上沿危险方向预设裂纹,采用有限元方法,于裂纹尖端构建奇异二维裂纹元,模拟裂纹扩展,分别计算随着裂纹扩展对应裂纹深度的应力强度因子,由此判断在内压与轴向过载作用下,裂纹只能以滑开方式失稳,最大允许裂纹深度可由临界应力强设因子确定。

关 键 词:稳定性分析  固体推进剂火箭发动机  推进剂药柱  裂纹扩展  有限元法  应力强度因子
文章编号:1001-4055(2002)04-0335-04
修稿时间:2001年9月10日

Stability analysis of the crack in solid rocket motor grain
MENG Shang yang,TANG Guo jin and LEI Yong jun.Stability analysis of the crack in solid rocket motor grain[J].Journal of Propulsion Technology,2002,23(4):335-338.
Authors:MENG Shang yang  TANG Guo jin and LEI Yong jun
Institution:Inst of Aerospace and Material Engineering, National Univ of Defence Technology, Changsha 410073,China;Inst of Aerospace and Material Engineering, National Univ of Defence Technology, Changsha 410073,China;Inst of Aerospace and Material Engineering, National Univ of Defence Technology, Changsha 410073,China
Abstract:A method to analyze the grain crack stability was presented The most dangerous section and the more dangerous points were determined by the three dimension viscoelastic finite element analysis of solid rocket motor grain Several cracks were preset along some directions in the more dangerous points, and the crack was simplified as the two dimension elastic crack because the most dangerous section is at the middle of the grain and motor work time is rather short The singular crack element and two dimension elastic finite element method were used to calculate the crack stress intensity factor The grain crack stability was discussed by stress intensity factor
Keywords:Solid propellant engine  Propellant grain  Crack propagation  Finite element method  Stress  intensity factor
本文献已被 CNKI 维普 万方数据 等数据库收录!
点击此处可从《推进技术》浏览原始摘要信息
点击此处可从《推进技术》下载免费的PDF全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号