铣削淬硬模具钢SKD11铣削表面质量试验研究
引用本文:景璐璐,沈中,陈明,胡祖光,励政伟,许辉,祝新发.铣削淬硬模具钢SKD11铣削表面质量试验研究[J].南京航空航天大学学报(英文版),2007,24(2):157-163.
作者姓名:景璐璐  沈中  陈明  胡祖光  励政伟  许辉  祝新发
作者单位:上海交通大学机械与动力工程学院,上海,200240,中国;上海工具厂,上海,中国
基金项目:国家自然科学基金 , 国家科技型中小企业技术创新基金 , 教育部跨世纪优秀人才培养计划
摘    要:为了对高效铣削淬硬模具钢SKD11的新型铣刀进行优选,对不同几何结构的铣刀加工得到的表面质量进行了分析.综合考虑了加工表面粗糙度、切屑微观形态、硬度及硬化层深度、残余应力分布和晶相组织结构变化等多方面因素,研究了不同铣刀的几何特性及其磨损特性对表面质量的影响.实验结果表明,前角5°,后角10°,刀尖圆弧半径为1 mm,铣刀螺旋角为45°的几何结构铣刀完成了表面完整性试验中.此外,在淬硬钢铣削加工中合理地选择加工参数可以获得0.4μm的表面粗糙度;采用合理的正前角可以抑制锯齿形切屑的产生.铣削淬硬模具钢能在加工表面产生残余压应力,通过增加铣刀后角和抑制后刀面磨损可以推迟加工表面软化现象的发生.

关 键 词:高速铣削  模具钢SKD11  表面质量  稳定性  high-efficiency  milling  hardened  steel  SKD  11  surface  integrity  stability  铣削  淬硬模具钢  表面  质量试验  研究  HARDENED  STEEL  TOOL  MILLING  INTEGRITY  SURFACE  occurrence  softening  increasing  clearance  compressive  residual  stress  induced  generation  depressed  reasonable  positive
文章编号:1005-1120(2007)02-0157-07
修稿时间:2006-06-272006-11-24

EXPERIMENT ON SURFACE INTEGRITY OF MILLING TOOL FOR HARDENED STEEL SKD11
Jing Lulu,Shen Zhang,Chen Ming,Hu Zuguang,Li Zhengwei,Xu Hui,Zhu Xinfa.EXPERIMENT ON SURFACE INTEGRITY OF MILLING TOOL FOR HARDENED STEEL SKD11[J].Transactions of Nanjing University of Aeronautics & Astronautics,2007,24(2):157-163.
Authors:Jing Lulu  Shen Zhang  Chen Ming  Hu Zuguang  Li Zhengwei  Xu Hui  Zhu Xinfa
Institution:1. School of Mechanical Engineering, Shanghai Jiao Tong University, Shanghai, 200240, P. R. China; 2. Shanghai Tool Works Co. Ltd. , Shanghai, P. R. China
Abstract:To evaluate the new designed cutting tools for high-efficiency milling of the hardened die steel SKD11,surface integrities of millers with different geometric structures are analyzed, considering the surface roughness, micrograph of chips, surface microhardness, residual stress and metallurgical texture of the surface layer. The in fluences of geometric characteristics of different cutting tools and their wear characteristics on the surface integrity are studied. Results show that the milling tool with rake angle; 5 of the hardened diesteel. The generation of saw-tooth chips is depressed when a reasonable positive rake angle is selected. And the compressive residual stress is induced on the machined surface in milling the hardened die steel. The occurrence of surface softening is postponed by increasing the clearance angle and reducing the tool flank wear.
Keywords:high-efficiency milling  hardened steel SKD 11  surface integrity  stability